Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.520 J/cm

@Temperature -10.0 °C
0.974 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene HJ640A PP
HJ640A Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation