Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.343233 - 0.441299 J/cm

@Temperature -10.0 - -10.0 °C
0.643016 - 0.826734 ft-lb/in

@Temperature 14.0 - 14.0 °F
Average value: 0.392 J/cm Grade Count:3
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..