Polymer Property : Izod Impact, Unnotched = 0.0900 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.0900 J/cm
0.169 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE002 PC
LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Izod Impact, Unnotched 0.0900 J/cm
0.169 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific)
LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber.