Mechanical Properties Metric English Comments
Izod Impact Notched 35.3 - 36.6 J
26.0 - 27.0 ft-lb
V-Notch
Latrobe Lescalloy® UT-18 VAC-ARC ; 2.125 in. round High Strength Alloy Steel
UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting..