Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Notched | 1.26 J | 0.930 ft-lb | |
Green Dot Terratek® BD 4015 Biodegradable Polymer Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the.. |