Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact | 20.3 J @Treatment Temp. 371 °C |
15.0 ft-lb @Treatment Temp. 700 °F |
Tempered for 2 hr |
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |
|||
Izod Impact | 20.3 J @Treatment Temp. 149 °C |
15.0 ft-lb @Treatment Temp. 300 °F |
Tempered for 2 hr |
EDRO #8 Premium 420 Stainless Mold Steel EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in.. |