Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 0.283 MPa @Temperature 400 °C, Time 1.80e+7 sec |
41.1 psi @Temperature 752 °F, Time 5000 hour |
time to produce 1% strain |
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |