Mechanical Properties Metric English Comments
Creep Strength 0.100 MPa

@Strain <=2.00 %,
Time 3.60e+6 sec
14.5 psi

@Strain <=2.00 %,
Time 1000 hour
Compressive; mid-term; DIN EN 1606
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Creep Strength 0.100 MPa

@Strain <=2.00 %
14.5 psi

@Strain <=2.00 %
Compressive; long-term; 50 years; DIN EN 1606
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..