Mechanical Properties Metric English Comments
Creep Strength 13.0 MPa

@Time 3.60e+6 sec
1890 psi

@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
Murtfeldt Murytal® C Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Creep Strength 13.0 MPa

@Time 3.60e+6 sec
1890 psi

@Time 1000 hour
stress leading to 1% elongation; 50% RH; ISO 899-1
Murtfeldt Murytal® C Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Creep Strength 13.0 MPa

@Time 3.60e+6 sec
1890 psi

@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Creep Strength 13.0 MPa

@Time 3.60e+6 sec
1890 psi

@Time 1000 hour
stress leading to 1% elongation; 50% RH; ISO 899-1
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..