Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 124.11 MPa @Temperature 538 °C |
18001 psi @Temperature 1000 °F |
|
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |