Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 0.160 MPa @Strain <=2.00 %, Time 3.60e+6 sec |
23.2 psi @Strain <=2.00 %, Time 1000 hour |
Compressive; mid-term; DIN EN 1606 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Creep Strength | 0.160 MPa @Strain <=2.00 %, Time 3.60e+6 sec |
23.2 psi @Strain <=2.00 %, Time 1000 hour |
Compressive; mid-term; DIN EN 1606 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |