Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 9.00 MPa | 1310 psi | |
Okulen® 2000 PE-UHMW, T OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |