Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 300 MPa @Temperature 600 °C, Time 3.60e+6 sec |
43500 psi @Temperature 1110 °F, Time 1000 hour |
|
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |