Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 26.0 MPa | 3770 psi | stress leading to 1% elongation; dry; ISO 899-1 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Creep Strength | 26.0 MPa | 3770 psi | stress leading to 1% elongation; 50% RH; ISO 899-1 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |