Creep Strength 6.00 - 24.0 MPa
870 - 3480 psi
Average value: 15.6 MPa Grade Count:15
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..