Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | >= 16.0 MPa | >= 2320 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Conditioned Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 16.0 MPa | >= 2320 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |