Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 200 MPa @Temperature 600 °C, Time 3.60e+6 sec |
29000 psi @Temperature 1110 °F, Time 1000 hour |
1% Creep Strain |
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthanum,...etc) which make the alloy particularly well designed for hig.. |