Mechanical Properties Metric English Comments
Creep Strength 3.20 - 13.0 MPa
464 - 1890 psi
Average value: 9.74 MPa Grade Count:29
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..