Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 13.0 MPa | 1890 psi | |
Okulen® 2000 PE-UHMW, CL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Creep Strength | 13.0 MPa | 1890 psi | 1% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |