Polymer Property : Creep Strength = 12.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Creep Strength 12.4 MPa

@Temperature 20.0 °C,
Time >=720000 sec
1800 psi

@Temperature 68.0 °F,
Time >=200 hour
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade
Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip..