Polymer Property : Creep Strength = 116 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Creep Strength 116 MPa

@Temperature 779.4 °C,
Time 180000 sec
16800 psi

@Temperature 1435 °F,
Time 50.0 hour
ATI Allegheny Ludlum Altemp® 263 Nickel-Based alloy
Characteristics: high strength up to 1500°F, oxidation resistance up to 2000°FInformation provided by Allegheny Ludlum