Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 7.50 MPa | 1090 psi | stress leading to 1% elongation; 50% RH; ISO 899-1 |
Murtfeldt Murylon® HT Nylon 46 The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir.. |