Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 65.0 MPa @Strain 3.50 % |
9430 psi @Strain 3.50 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |