Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 1705 MPa @Temperature 23.0 °C |
247300 psi @Temperature 73.4 °F |
Autoclave Cured; [0°]16 |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |