Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 1611.1 MPa @Temperature 22.8 °C |
233670 psi @Temperature 73.0 °F |
Flexure Long; 30 min @ 250°F; prEN 2563 |
Hexcel® HexPly® EF02 Epoxy Curing System after THR 120 EF01 S50 37% Curing Cycle Information provided by HexCel |