Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 12.0 MPa @Temperature 232 °C |
1740 psi @Temperature 450 °F |
Autoclave Cured; [90°]16; Wet condition |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |