Mechanical Properties Metric English Comments
Flexural Yield Strength 115 MPa

@Strain 3.50 %
16700 psi

@Strain 3.50 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66