Mechanical Properties Metric English Comments
Flexural Yield Strength 107 MPa

@Temperature 177 °C
15500 psi

@Temperature 351 °F
T300 (6K); [90°]16
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form
Fiber: T300-12K, IM7-12KInformation provided by HexCel