Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 90.0 MPa @Strain 3.50 % |
13100 psi @Strain 3.50 % |
Conditioned; ISO 178 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Yield Strength | 90.0 MPa @Strain 3.50 % |
13100 psi @Strain 3.50 % |
Conditioned; ISO 178 |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Yield Strength | 90.0 MPa @Strain 3.50 % |
13100 psi @Strain 3.50 % |
Conditioned; ISO 178 |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |