Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 122 MPa @Strain 3.50 % |
17700 psi @Strain 3.50 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |