Mechanical Properties Metric English Comments
Flexural Yield Strength 117 MPa

@Temperature 23.0 °C
17000 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin
HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding..