Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.06 J/cm² | 9.80 ft-lb/in² | EN ISO 179 |
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |