Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.80 - 17.0 J/cm²
18.1 - 80.9 ft-lb/in²
Average value: 10.1 J/cm² Grade Count:6
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..