Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.29 - 8.49 J/cm² @Temperature -30.0 - -30.0 °C |
39.5 - 40.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 8.39 J/cm² Grade Count:2 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |