Polymer Property : Charpy Impact Unnotched = 8.185 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.720 J/cm²

@Temperature 23.0 °C
8.185 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eU
FKuR Kunststoff Terralene® WF 5525 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..