Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.367 J/cm² | 35.08 ft-lb/in² | |
PSM Industries Ferro-TiC® PK Maraging Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Comb.. |