Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.00 - 6.90 J/cm² @Temperature -30.0 - 30.0 °C |
19.0 - 32.8 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 5.95 J/cm² Grade Count:13 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |