Polymer Property : Charpy Impact Unnotched = 6.80 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.30 - 6.80 J/cm²
10.9 - 32.4 ft-lb/in²
Average value: 4.31 J/cm² Grade Count:17
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Charpy Impact Unnotched 4.00 - 6.80 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 32.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.77 J/cm² Grade Count:3
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..