Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.36 J/cm²
6.47 ft-lb/in²
ISO 179-1
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound
Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak..