Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.12 J/cm² | 29.1 ft-lb/in² | |
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Dry) Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:.. |