Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.4 J/cm² | 49.5 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |