Polymer Property : Charpy Impact Unnotched = 44.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 9.27 J/cm²
44.1 ft-lb/in²
ISO Data, Low Temp
Dow AIM® 4800 High Impact Styrenic Resin
AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur..