Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.80 - 3.80 J/cm²

@Temperature -20.0 - -20.0 °C
18.1 - 18.1 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 3.80 J/cm² Grade Count:1
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Charpy Impact Unnotched 3.80 - 3.80 J/cm²

@Temperature -30.0 - -30.0 °C
18.1 - 18.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.80 J/cm² Grade Count:1
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..