Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 25.2 J/cm² | 120 ft-lb/in² | ISO 179 |
GEHR Plastics PVDF Polyvinylidene Fluoride Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |