Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.868 J/cm² | 13.65 ft-lb/in² | ISO 179-1:2007 |
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing Processed by selective laser sintering (SLS). Windform® SP is a deep black composite polyamide that is a “Top” level material within the polyamide Windform® materials for additive manufacturing.. |