Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.10 - 13.0 J/cm² @Temperature -40.0 - 30.0 °C |
5.24 - 61.9 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 4.94 J/cm² Grade Count:33 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |