Polymer Property : Charpy Impact Unnotched = 12.33 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.589 J/cm²
12.33 ft-lb/in²
PSM Industries Ferro-TiC® CS-40 Martensitic Stainless Steel
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.High..