Mechanical Properties Metric English Comments
Charpy Impact Unnotched 10.8 J/cm²
51.4 ft-lb/in²
ISO 179/1EA-1993
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal ..
Charpy Impact Unnotched 10.8 J/cm²
51.4 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, Conditioned
Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used..