Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.1 J/cm² | 48.1 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |