Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.814 J/cm² | 8.633 ft-lb/in² | ISO 179-1:2007 |
CRP Technology Windform® LX 2.0 Polyamide Composite Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability .. |